The agent can produce a non-metallic coating on the surface of the steel wire. This coating helps the formation of the lubricating film, greatly improves the lubrication and deformation resistance of the metal surface, and has good rust resistance.
Nickel-free, good thermoplasticity, suitable for drawing of steel wire ropes and steel strands. Scaled film has good ductility and low mold loss, although the compression ratio is high.
This product is aluminum or aluminum alloy spray paint or sprayed aluminum surface phosphating agent. The aluminum and aluminum alloy workpieces treated by this drug can form a colorless or yellowish phosphating coating on the surface, and can improve the adhesion and corrosion resistance of the surface coating (painting, spray) of aluminum and aluminum alloy workpieces.
Process parameters
Process parameters
Tank maintenance
Instructions
General process
Packaging and storage
Packaging and storage
Temperature 75-85 C
Time 5-10 min
Total acidity 55~75pt
Free acidity 8〜12pt
Temperature Normal temperature - 45℃
P H value 2.6-3(Determined with 0.5-5 precision test paper)
Time 5-8 min
EN84-2:40~50kg/T (4-5%)
During use, as the solution is continuously consumed, the concentration will continue to decrease, and it is only necessary to control the pH and adjust the bath concentration. The bath should be replaced when the aluminum ion content in the solution exceeds 2 kg/ton.
— Use 10-15% to form a bath; then heat the bath to above 75 °C, then add 0.4~l% c4 Cuihua, you can scale the wire (round)
— In the production process, the supply agent is added according to the consumption of 40~50g/m2;